On a Sierra series tube using Polyester Resin and the Resin Saver mold.
Heated PR in warm water to a consistency of water while stirring in catalyst for 2 minuets.
Removed any air bubbles until gelled and placed in warming chamber for 6 hours to cure and gas-off.

Tube painted with Krylon FUSION White spray paint with 2 Pheasant feathers and 2 tied flies attached to the tube.

Les

xzn04.jpg
 
Signed-In Members Don't See This Ad
Warming Chamber

that looks great! cant wait to see it turned!!What is the so called warming chamber?

This is the Warming Chamber is use to cure and gas-off all my Pr castings.
Thanks Branden - ( penl8the ) for your help putting this together.