Here are the results of my 3rd attempt at making fordite. I used a hot plate to heat the mold from below to continuously flow out the powder as I sprinkled on each layer (56 total layers of powder coat powder). I did not find any noticeable bubbles this time. If there is any interest in buying blanks like this let me know and I will make a bigger hot plate so I can use a larger mold (9x12.75 inches).
There are 7 different colors of powder used to make these.